So a Saturday and part of a Sunday finds the port side hull clad in nice smooth glass. Again, peel ply tops the epoxy and glass and makes it possible to work the resin out and helps insure a good bond between the foam and the glass. My process goes like this.....smoothe the foam, skim coat with micro/epoxy mix to fill the foam surface. roll on a good wet coat of epoxy, lay down the glass, roll on another good wet coat of resin, top with peel ply and work the layers down with a bondo spreader from stem to stern.